ds-凯发k8官方网娱乐官方

it can be directly put into mixing tanks to produce high-viscosity asphalt mixture, and can also be added into asphalt to produce high-viscosity modified asphalt for paving permeable asphalt pavement.

product details

product introduction
it can be directly put into mixing tanks to produce high-viscosity asphalt mixture, and can also be added into asphalt to produce high-viscosity modified asphalt for paving permeable asphalt pavement.

型号

使用方法

添加量(占沥青质量)/%

温度

/

添加方式

ds-dsmh

直投拌缸

8~12

集料185~190

干拌15s后,加入沥青湿30s以上

 

 

生产高黏改性沥青

 

沥青165~185

sbs改性沥青生产工艺制得高黏改性沥青后与集料拌和